Protoyping Center
Introduction to Prototyping Preparing circuitry artwork
Boards Exposure
Developing Etching


Step by Step Process

Obtain Exposure and Photofabrication Kits Peel back protective backing off of presensitized copper clad board Place artwork on board Place acrylic weight on artwork and board Expose 5 min. with Exposure Kit Mix Developer 10:1 with water Brush developer over board (1 - 2 min) Rinse Etch with Ferric Chloride (4 - 5 min) Rinse